The boronizing process to titanium is developed to get high quality diaphragms for loudspeakers. A titanium diaphragm is buried in a mixed power of boron, carbon, and sodium carbonate, and heated. By this process, titanium borides in the form of TiB and TiB2 are obtained at the diaphragm surface. Ten minutes of treatment at 1,200 degree Centigrade to a 25µm thickness titanium diaphragm gives a Young's modulus of 2.7 x 1011 N/m2, density of 4.23 x 10 kg/m3 and boronized depth of 5 µm. The E/p of boronized titanium reaches to about three times of titanium. Using high Young's modulus bornonized titanium diaphragms, loudspeakers with wide-range, low-distortion, and excellent transient response can be realized.
Authors:
Yamamoto, Takeo; Tsukagoshi, Tsunehiro; Tanaka, Fujio; Tohma, Teruo; Kimura, Masami
Affiliation:
Pioneer Electronic Corporation, Saitama, Japan
AES Convention:
63 (May 1979)
Paper Number:
1494
Publication Date:
May 1, 1979
Click to purchase paper as a non-member or you can login as an AES member to see more options.
No AES members have commented on this paper yet.
To be notified of new comments on this paper you can subscribe to this RSS feed. Forum users should login to see additional options.
If you are not yet an AES member and have something important to say about this paper then we urge you to join the AES today and make your voice heard. You can join online today by clicking here.